The 24-year clinical performance of porcelain laminate veneer restorations bonded with a two-liquid silane primer and a tri-n-butylborane-initiated adhesive resin

Mitsuo Nakamura, Hideo Matsumura
2014 Journal of Oral Science  
This report describes the bonding technique and clinical course of porcelain laminate veneer restorations applied to discolored maxillary incisors and canines. The patient was an 18-yearold woman, and tooth reduction was limited to the enamel. Laminate veneer restorations were made with a feldspathic porcelain material (Cosmotech Porcelain). After try-in, enamel surfaces were etched with 65% phosphoric acid gel, and a tri-nbutylborane-initiated resin (Super-Bond C&B) was applied as a bonding
more » ... nt. The inner surface of the restorations was etched with 5% hydrofluoric acid gel (HF Gel) and treated with a two-liquid silane primer (Porcelain Liner M), after which the Super-Bond resin was applied. Each restoration was seated with a dual-activated composite luting agent (Cosmotech Composite). After 24 years and 8 months, the restorations are functioning satisfactorily. The luting system and bonding technique described in this report are an option for seating laminate veneer restorations made of silica-based tooth-colored ceramics. (J Oral Sci 56, 227-230, 2014)
doi:10.2334/josnusd.56.227 pmid:25231150 fatcat:jgsx4vmwfrfqzomjdj2cushznm