A copy of this work was available on the public web and has been preserved in the Wayback Machine. The capture dates from 2018; you can also visit the original URL.
The file type is application/pdf
.
On the Spot Formation during Gas-Tungsten-Arc Welding of 18-8 Stainless Steel Thin Sheet
18-8ステンレス鋼薄板のTIG溶接中に生ずるスポット状欠陥について
1970
JOURNAL OF THE JAPAN WELDING SOCIETY
18-8ステンレス鋼薄板のTIG溶接中に生ずるスポット状欠陥について
Formation of spot defect is often observed on the surface of weld bead during the Tungsten inert gas welding of 18-8 stainless steel thin sheet.
doi:10.2207/qjjws1943.39.6_540
fatcat:ylccmn34ybhzpf62hbvfnibl6i