A copy of this work was available on the public web and has been preserved in the Wayback Machine. The capture dates from 2018; you can also visit the original URL.
The file type is application/pdf
.
Evaluation of wear performance of cryogenically treated Vanadis 4 Extra tool steel
2016
Kovové materiály
In this study, the wear performance of cryogenically treated cold-work tool steel (Vanadis 4 Extra) samples was evaluated in the light of some sliding wear tests. For this purpose, the samples were cryogenically treated for different durations (0, 1, 12, and 24 h) at deep cryogenic temperature (-145 • C). A tempering process was performed at two different temperatures (175 and 525 • C) for 2 h. The wear experiments were carried out in a ball-on-disk tester, by applying two loads of 10 and 20 N
doi:10.4149/km_2016_3_195