Lifetime Analysis of the ITER First Wall and Divertor Plates

R.F. Mattas
1989 Fusion Technology  
The performance of the ITER first wall and divertor plate is analyzed using a 1-D lifetime code which includes the effects of radiation damage and surface erosion. The materials considered for the first wall are solution annealed and 20$ cold-worked Type 316 stainless steel. The materials considered for the divertor plate are H-451 graphite bonded to a Cu-0.5 Be-2 Ni heat sink. The primary conclusion is that it is crucial to include radiation effects for obtaining realistic predictions of