Improving Shale Inhibitive Performance using Methyl Glucoside (MEG) in Potassium Chloride Mud

Issham Ismail, Ahmad Shamsul Izwan Ismail, Nur Suriani Mamat, Muhamad Khairul Amin Muhtar
2014 Jurnal Teknologi  
Oil-based mud has shown a commended performance over the years in mitigating borehole instability especially when penetrating through a reactive shale zone which is known to have swelling and dispersion problems. However, the strict environmental regulations worldwide have limited the use of oil-based mud. Therefore the methyl glucoside, known as MEG, a specially formulated water-based mud has been introduced where its performance is close to the oil-based mud. This project studied the effect
more » ... using MEG in potassium chloride (MEG/KCl) mud in controlling shale swelling and dispersion. Five different concentrations (0, 5, 15, 25, and 35% by weight) were used in the hot rolling dispersion test. Besides, the rheological properties and fluid loss control were also tested as per the American Petroleum Institute -Recommended Practice -13B (2009). The results showed that MEG/KCl mud was capable of improving the shale inhibitive performance to mitigate the shale swelling and dispersion problems. The higher concentration of MEG used such as 25% and 35%, the less shale would swell or disperse. However, the effectiveness of MEG was corresponding with clay content present in the shale. Abstrak Lumpur dasar minyak telah menunjukkan prestasi yang baik sepanjang masa dalam mengurangkan masalah ketidakstabilan lubang telaga apabila menembusi zon syal reaktif yang memang terkenal dengan masalah pembengkakan dan penyerakan syal. Namun begitu, peraturan alam sekitar yang ketat menyebabkan penggunaan lumpur dasar minyak semakin terhad. Sehubungan dengan itu, metil glukosida atau dikenal sebagai MEG, sejenis lumpur dasar air yang dirumus khas telah diguna pakai, dengan prestasinya hampir setanding dengan lumpur dasar minyak. Projek ini dilaksanakan untuk mengkaji kesan penggunaan MEG dalam lumpur kalium klorida (MEG/KCl) bagi meningkatkan kawalan terhadap pembengkakan dan penyerakan syal. Lima kepekatan yang berbeza (0, 5, 15, 25, dan 35% berdasarkan berat) telah digunakan dalam prosedur ujian penyerakan putar panas. Di samping itu, sifat reologi dan sifat kawalan kehilangan bendalir turut diuji berdasarkan American Petroleum Institute -Recommended Practice -13B (2009). Keputusan kajian menunjukkan bahawa lumpur MEG/KCl mampu mengurangkan masalah pembengkakan dan penyerakan syal. Semakin tinggi kepekatan MEG yang digunakan, misalnya 25% dan 35%, maka semakin berkurang masalah pembengkakan serta penyerakan syal. Namun begitu, keberkesanan MEG adalah bergantung pada kandungan lempung yang wujud dalam syal. Kata kunci: Ujian penyerakan putar panas; metil glukosida; lumpur dasar minyak; pembengkakan syal; lumpur dasar air
doi:10.11113/jt.v68.2070 fatcat:ve5mwoqumveojm6wdrrux5iu5e