A copy of this work was available on the public web and has been preserved in the Wayback Machine. The capture dates from 2020; you can also visit the original URL.
The file type is application/pdf
.
THE DEFORMATION OF AZ31 MAGNESIUM ALLOY DURING WARM CONSTRAINED GROOVE PRESSING
2019
Acta Metallurgica Slovaca
A magnesium alloy AZ31 as plate of dimensions (60 x 60 x 3) mm has been constrained groove pressed (CGP) four deformation passes (16 pressings) at 250 oC by simulation and expremental. On the basis of the analysis of calculation results about the deformation distribution in the alloy AZ31 workpiece the mechanism for its microstructure evolution during the severe plastic deformation (SPD) process was partly clarified. On the other hand, deformation heterogeneity distribution developed in plate
doi:10.12776/ams.v1i1.1218
fatcat:n5mkrtpourefzfkgdbys3hb2ny